DEV Community

Asher Hu
Asher Hu

Posted on Originally published at hezidesign.com

Weld lines sit where the gate puts them: fix location before process

A weld line's position is decided by the gate; its depth is decided by melt and mould temperature. With the same tool and the same gate, the line is always in the same place. Changing resin or tuning the machine makes it fainter, never moves it. So the order is: first judge whether the position is acceptable; if not, move the gate; only then discuss how to hide it.

Position and depth are two different problems with two different routes. A weld line forms where two flow fronts meet after both have cooled, so the interface never fuses. When the fronts meet within 20°C of each other the line is essentially invisible; above 40°C it shows as a dark line that neither polishing nor paint will hide. Position follows the geometry between gate and cavity - shift the gate by 10mm and the line moves to another edge. Injection speed, melt temperature and mould temperature only change how deep and how wide it is.

Think of the cavity as a pool. Resin enters at the gate, and wherever the two fronts meet, that is where the weld line sits. This is why hours of tuning leave the line exactly where it started.

There are only two ways to move it: relocate the gate, or change the part split. The cheapest moment is during tool design - move the injection point on the drawing and change one insert later. Once the tool is cut, you are modifying the cavity block and paying for it in money and weeks. We issue a weld-line prediction drawing as part of the structural review specifically to pull this decision forward.

When the position is acceptable, four parameters reduce depth. Venting comes first because it costs almost nothing: add vents at the meeting point, 0.02-0.03mm deep. Without venting the gas pushes back at the confluence, the line deepens and may scorch. On a display housing project, two vent inserts alone dropped the visible line by a whole grade. Melt temperature next, up to 10°C above the supplier's recommended value - beyond that, degradation and yellowing. Mould temperature of 60-80°C, higher for clear parts, at the cost of longer cooling. Injection speed mid-to-fast, with a deceleration just before the fronts meet, because too fast traps gas and too slow lets the front cool.

Whether an appearance part may carry a weld line is a graded question. Clear parts and high-gloss moulded-in-colour parts: not acceptable at all. Matte, textured or dark parts: acceptable if it is invisible at 300mm under the specified lighting. We write viewing distance and lighting into the acceptance clause instead of "no visible weld line", which cannot be measured. If the line sits somewhere unacceptable and the gate cannot move, hide it - route the confluence to the parting line, into the texture, or under a decorative part. Painting a weld line is the least reliable option: adhesion over the line is poor and the paint fails there first.