When two plastic shells meet, the joint is usually a lip: a tongue on one half running into a groove on the other. Three numbers decide whether the seam is tight or visible, and all three have to be settled on the drawing rather than tuned by an assembler's feel. The single-side clearance is normally 0.05 to 0.1 mm, the insertion depth 1.5 to 3 mm, and the entry lead-in angle 15 to 30 degrees.
Where does the clearance band come from? Injection moulding itself. Small parts hold about plus or minus 0.05 mm across production batches, medium and large parts about 0.1 mm. Set the clearance below the natural variation and a portion of assemblies simply will not close; set it above twice the variation and the parts rock against each other and the flush surface is gone. On the thickness direction, leave 0.05 mm as well: a lip that bottoms out early pushes the shell face into a visible bulge around it.
The second thing people get wrong is purpose. A lip is a locating feature, not a seal. Shrinkage, warpage and assembly stress will open a 0.05 mm channel along the joint no matter how snug the drawing looks, so waterproofing belongs to gaskets or adhesive. Locating wants no movement but free assembly; sealing wants compression. The two goals pull the tolerance in opposite directions, and a lip asked to do both fails at both. If the brief says the seam must be invisible, the right move is not zero clearance, which only tanks yield as the mould wears, but hiding the seam: a stepped offset, or a fine groove that redirects the eye. Neither changes the fit.
Assembly order matters too: lip first, snap second. If the snaps engage first, the lip enters crooked and its edge whitens or cracks. Keep the snap engagement direction parallel to the lip insertion direction; a side-then-down assembly loads the lip in shear, and that failure is visible on the drawing without waiting for a prototype shot.
Finally, when a step appears between the halves, tightening the lip is usually the wrong fix. The step is the sum of three tolerances: lip clearance, the parting-line height difference of the two moulded faces, and how the locking force distributes after closure. Measure in that order, parting line first, clearance second, locking last. In one real case the step hovered near 0.2 mm no matter what the lip did; the upper shell carried 0.08 mm of mould machining error on its parting line, and after the tool was hand-fitted back inside 0.02 mm, the step stabilised at once. Parting line is a tooling problem, clearance is a drawing problem, locking is a process problem, and the three fixes sit in very different price ranges. For acceptance, write the method into the clause: no visible step at 300 mm viewing distance under 45-degree side light beats a bare number, because step perception depends heavily on illumination angle.