Two-shot peeling: check 0.3–0.8 mm groove, 60–80 C mold entry, drop-line offset

Two-shot moulding usually fails in one visible way: the soft overmould lifts at an edge, or the part splits along the seam in a drop test. The reflex answer is that the glue is bad, but there is no glue. Adhesion between the hard and the soft shot comes from geometry, temperature and placement, and all three are decided while the part is still a drawing.

The first check is mechanical interlock. On many drawings the parting line is two curves with a note saying "two-shot here". In the tool that becomes two flat faces pressed together, held by molecular entanglement and not much else. It passes a pull test when new and opens after a few thermal cycles. The fix is a groove around the boundary of the first shot, 0.3 to 0.8 mm deep, which the second shot fills and locks. To separate the two materials, a drop load now has to shear that lock. Width to depth matters: too narrow and the melt will not fill the groove, too wide and it does not lock. This is also why the hard side needs at least 1.2 mm of wall at the boundary - below that the groove cannot be cut at all.

The second check is shrinkage mismatch. Hard PC/ABS shrinks around 0.5 per cent; soft TPE or silicone can reach 1.5 to 2 per cent. If the first-shot part is cold when the second shot goes in, the soft skin shrinks against a cold surface and the interface takes shear stress, which shows up as lifted corners. The answer is not a different material, it is temperature: keep the first-shot surface at 60 to 80 degrees C on entry to the second tool, through inter-station insulation on a rotary mould, a shorter cycle between the two shots, or a higher second-shot tool temperature. At the trial stage this is the fastest variable to test: if the edges lift, feel the first-shot part before blaming the design.

The third check is where the line sits. The seam is the weakest ring on the part. On a handheld device we saw, the boundary ran along the middle of the side face and cracked at the seam in a 1.2 metre drop. Moving the line up, more than 3 mm clear of the top corner so the impact edge lands in solid hard plastic, added a visible line to the appearance and one grade to the strength. No process change could have saved the first layout.

Two practical notes from quotes. Choosing between true two-shot and a separate overmoulding operation comes down to volume and registration: the rotary tool holds under 0.05 mm and costs more, a second mould is cheaper and typically lands at 0.1 to 0.2 mm, which is fine for a few thousand pieces and not fine for tens of thousands with a crisp seam. And plasticiser bloom - a tacky, dust-attracting soft surface - is a material ageing problem, so ask the supplier for the surface condition after 168 hours at 85 degrees C and 85 per cent RH before signing off the compound. Changing powder-free is cheap at quotation stage and expensive after the tool is cut.