Warping and poor adhesion can both lift a part off the bed, but they have different causes, and a fix for one may do nothing for the other. Before changing anything, work out which one you have.
Read the symptom first
If the corners or edges start to lift while the part grows, it can be warping. If the first layer does not stick from the start, or the base starts to come loose in the first layers, it is an initial adhesion problem. These signs help separate the two, though they are not always enough on their own.
| What you see | What to check first |
|---|---|
| Corners lift while printing | The material, the bed temperature, drafts around the printer |
| The base never sticks to the plate | Plate cleanliness, the plate selected in the slicer, nozzle distance |
Why the part comes loose
Shrinkage and temperature
Prusa explains warping as usually the result of a sudden difference between the melting temperature at the nozzle and the ambient temperature. The plastic shrinks and warps, mostly with high-temperature materials such as PC Blend, ASA or ABS, and on large objects. Creality's table rates the risk as low for PLA, medium for PETG and high for ABS, and suggests avoiding strong cooling fans with PETG.
The room matters too. Prusa says an open window or an AC unit near the printer will increase the occurrence of warps.
Initial adhesion
Here the part never gets stuck. Flashforge lists oil stains on the build plate, a damaged or worn plate and an improper nozzle distance after leveling as causes. On Bambu Lab printers there is a common one on top of that: picking a plate type in the slicer that is not the one installed. Bambu Lab notes that the same material is usually printed at different bed temperatures depending on the plate, so the wrong selection can leave the adhesion short.
What to try, simplest first
Start with the cheap checks before changing print settings or parts. You do not need all of them, only the ones that match your problem.
Clean the plate the way its maker says. Bambu Lab strongly recommends washing its plates with hot water and detergent before printing, without touching the surface afterwards. For its steel sheets, Prusa gives isopropyl alcohol of 90% or more for smooth, satin and textured ones, warm water with dish soap when adhesion fades over time, and acetone only on smooth PEI, about once a month. It says never to use acetone on textured or satin sheets.
Check the plate is right and that the slicer knows it. Two checks: the surface suits the material, and the plate type chosen in the slicer matches the one installed.
If the part still will not stick, consider glue stick. Try a brim first, covered below. A glue stick can do two jobs: help the part stick, or act as a separation layer when a material grips so hard it could damage the plate. Prusa says a thin layer of glue stick applied to the cold steel sheet can do both. It recommends a separating agent for PETG, ABS, ASA, XT and CPH on smooth PEI, says it is not needed for PLA in its experience, and says it may be advisable for nylon, PETG, PC, ABS and ASA. Prusa also says: do not put super glue on your sheet.
Check leveling and the first layer. Follow the manufacturer's leveling procedure and make sure the nozzle distance lets the first layer lay down properly. Do not squash it too much either: Prusa notes that with PETG or PC, adhesion can get strong enough to damage a PEI sheet.
Match the bed temperature to the filament. Use the range your filament maker publishes, within the limits of your printer and plate. Prusa suggests raising the bed by 5 to 10 °C with new materials that do not stick, and Creality gives roughly 50 to 60 °C for PLA and 90 to 110 °C for ABS, as general figures. Those are not universal values. The bed temperature is not the chamber temperature.
Print the first layer slower. Prusa suggests about 75% of normal speed for the first three layers. The right value depends on the printer and the material.
If the edges lift, try a brim. A brim is a set of lines the slicer prints around the base to widen its contact area with the plate. Prusa says to consider the brim before adding extra adhesion materials to the bed.
For ABS and ASA, consider an enclosed printer. Prusa says high-temperature materials generally need a higher ambient temperature not to warp, and that if you print them most of the time you should consider an enclosure. It adds that printing PLA or PETG in an enclosure might not be a good idea, because those materials need a lot of print cooling, which is harder to achieve with a higher ambient temperature. Creality also suggests enclosing the printer to keep temperatures uniform and avoid drafts.
Sources
Everything above comes from the manufacturers' own documentation:
- Prusa, "Warping" and "First layer issues", Prusa Knowledge Base (consulted 03/11/2026 and 11/11/2026).
- Bambu Lab, "First layer not sticking", Bambu Lab Wiki (consulted 03/11/2026 and 11/11/2026).
- Creality, "3D Print Warping: What Causes It, How to Fix It, and How to Prevent It", Creality blog (consulted 03/11/2026 and 11/11/2026).
- Flashforge, "Troubleshooting: Equipment Usage Issues" for the Adventurer 5M, Flashforge documentation (consulted 03/11/2026).
The full version, in Spanish and with compatible parts for specific printers, is at laprimeracapa.es.