Stringing is the cobweb of thin strands left between separate parts of a print, or on its surface. Bambu Lab describes it as thin filaments unintentionally pulled out when molten filament seeps from the nozzle during travel moves. Oozing is a related defect: material keeps seeping out when the nozzle should not be extruding, and it piles up on the part or the nozzle. Bambu Lab says the two usually share causes, mostly excessive extrusion at the nozzle, damp filament or improper retraction settings.
Read the symptom first
| What you see | What to check first |
|---|---|
| Thin strands between separate parts | Retraction, temperature, the distance between the areas being printed |
| Strands with popping or hissing during extrusion | Whether the filament is wet |
| Blobs or buildup on the part or the nozzle | Temperature and the state of the nozzle |
Why strands appear
Wet filament
Polymaker says that if you hear pops or sizzling while extruding, that is water vapor escaping, and that wet filament creates stringier prints because steam causes inconsistent extrusion and little wisps between parts. Bambu Lab explains the mechanism: the moisture vaporizes when heated and the molten material bursts and flows abnormally. For Bambu Studio, it adds that damp filament is more prone to stringing and oozing, and that this usually cannot be fully solved by adjusting retraction alone: dry the filament first, then adjust retraction.
Retraction and travel moves
Between one area of the part and another, the head travels without printing. To limit the flow on that trip, the slicer pulls back some filament, which is retraction. If retraction is too short, molten material keeps coming out during the trip and can leave a strand along the way. Parts with separate areas are more prone to strands, and so are several parts spread across the bed, because the head covers more distance without printing. Bambu Lab lists long travel distances with insufficient retraction as the second cause after damp filament. The right value depends on the extruder type, the material and the printer.
Nozzle temperature
Bambu Lab says an excessively high nozzle temperature reduces the viscosity of the molten material and leads to abnormal extrusion. Prusa also lists a high temperature among the causes.
The nozzle itself
Prusa says that if you print for a long time with one type of filament, such as PET-G, the filament can leave a thin layer in the nozzle, which can cause stringing, so it recommends cleaning the nozzle thoroughly before printing. Bambu Lab adds that a nozzle that is too large, or worn, is another cause, and recommends a configuration that matches the real nozzle and replacing a worn one.
The material
Polymaker says PETG is known for being stringy, so it will be difficult to get rid of all of it. Flashforge adds that stringing alone does not prove PETG is wet, because nozzle temperature, travel speed, retraction and cooling can create similar defects. Bambu Lab lists low-density filaments such as PLA Aero as another cause: they contain internal voids and gases, including moisture, and if the temperature and flow ratio are not lowered they string more.
What to try
Start with the profile recommended for your printer and filament. On Prusa printers those are the official PrusaSlicer profiles.
If strings remain with that profile, try a different spool than the one causing the problem. That is Prusa's suggestion, because the filament might have gathered moisture, and Flashforge suggests drying it or replacing it with a newly unpacked filament. If the strands disappear with another spool, dry the first one before touching any setting. Bambu Lab recommends drying the filament before printing and storing it in a sealed container with desiccant.
Once the spool is dry, what remains is retraction, temperature and travel moves. Change them in small steps and check the result before the next change.
On retraction, you can raise the length or the speed a little, up to a limit, because too much can cause clogs. Bambu Lab generally recommends keeping the length no greater than 2 mm. Prusa gives a maximum of 2 mm for the MK2.5/S and MK3/S/+, while the MINI, which has a Bowden extruder, defaults to 3.2 mm. Those values belong to the models named, so for another printer use the manufacturer's documentation.
On temperature, Prusa and Creality suggest lowering the nozzle temperature by 5 to 10 °C, within the range recommended for the filament.
On travel moves, Bambu Lab suggests reducing the spacing between models and enabling "Avoid crossing wall". Prusa has the equivalent "Avoid crossing perimeters" and "Only retract when crossing perimeters".
Removing strings from a finished print
Prusa suggests passing a heat gun set to about 200 °C over the strings for one or two seconds to melt them, and warns that leaving the heat source on the model for longer may deform the part.
Sources
Everything above comes from the manufacturers' own documentation:
- Prusa, "Stringing and oozing", Prusa Knowledge Base (consulted 04/11/2026 and 11/11/2026).
- Bambu Lab, "Stringing and oozing" and the Bambu Studio retraction parameters, Bambu Lab Wiki (consulted 04/11/2026 and 11/11/2026).
- Polymaker, "Wet Filament" and "Polymaker Material Print Tips", Polymaker Wiki (consulted 04/11/2026 and 11/11/2026).
- Flashforge, "PETG drying temperature", Flashforge blog (consulted 04/11/2026 and 11/11/2026).
- Creality, "3D Print Retraction Guide: Fix Stringing & Improve Quality", Creality store blog (consulted 04/11/2026).
The full version, in Spanish and with compatible parts for specific printers, is at laprimeracapa.es.